This was the UHPGP mortar with 127-137 MPA (almost 19000-19600 psi) obtained using crushed granite or crushed basalt or wastes from zirconium aluminates from used refractory bricks
This was the UHPGP mortar with 127-137 MPA (almost 19000-19600 psi) obtained using crushed granite or crushed basalt or wastes from zirconium aluminates from used refractory bricks
We are engaged in research, development, and production of geopolymer-based sustainable construction materials, alongside the equipment to mix and print them.